Adhesive Strength in Dentin Conditioned with 18% Ethylenediaminetetraacetic Acid versus 35% Phosphoric Acid: In Vitro Study with 1-Year Artificial Aging
Average rating
Cast your vote
You can rate an item by clicking the amount of stars they wish to award to this item.
When enough users have cast their vote on this item, the average rating will also be shown.
Star rating
Your vote was cast
Thank you for your feedback
Thank you for your feedback
Authors
Alcántara-Obispo, EstherSantander-Rengifo, Flor
Ladera-Castañeda, Marysela
López-Gurreonero, Carlos
Castro Pérez-Vargas, Antonieta
Cornejo-Pinto, Alberto
Cervantes-Ganoza, Luis
Cayo-Rojas, César
Issue Date
2022-10-01Keywords
adhesive strengthbulk fill resin
ethylenediaminetetraacetic acid
phosphoric acid
resin composite
shearing
Metadata
Show full item recordPublisher
MDPIJournal
PolymersDOI
10.3390/polym14204291Additional Links
https://www.mdpi.com/2073-4360/14/20/4291Abstract
The success and longevity of a resin composite restoration is determined by its good bonding to the tooth structure, with the adhesion being a challenge to dentin due to its complexity and structural heterogeneity. The present study aimed to compare the adhesive strength of dentin conditioned with 18% ethylenediaminetetraacetic acid (EDTA) versus 35% phosphoric acid (H3PO4) in human premolars. Materials and Methods: This in vitro experimental study was performed on 40 human premolars. The occlusal thirds were sectioned and randomly placed into four groups according to the type of dentin conditioning: Group 1 (control), Group 2 (18% EDTA), Group 3 (35% H3PO4) and Group 4 (18% EDTA plus 35% H3PO4). Then, 10,000 thermocycles between 5 +/− 2 °C and 55 +/− 2 °C were applied. Adhesive strength was tested by shearing with a digital universal testing machine at a crosshead speed of 0.75 mm/min. The values obtained were analyzed in megapascals (MPa). The mean and standard deviation were used as measures of central tendency and dispersion. In addition, a one-factor intergroup ANOVA test was applied with Tukey’s post hoc test considering a significance level of p < 0.05. Results: The 18% EDTA and 18% EDTA plus 35% H3PO4 showed significantly higher adhesive strength compared to the control group that did not receive dentin conditioning (p = 0.047 and p < 0.001, respectively). However, the group conditioned with 18% EDTA did not present significant differences compared to the group conditioned with 35% H3PO4 (p = 0.997). In addition, the group conditioned with 18% EDTA plus 35% H3PO4 showed significantly higher adhesive strength compared to the groups conditioned with 18% EDTA (p = 0.002) and 35% H3PO4 (p = 0.001). Conclusion: The adhesion of bulk fill resin composite to dentin was favorable when preconditioning was performed using 18% EDTA followed by 35% H3PO4. In contrast, when both etchants were used separately, the bulk fill resin composite showed similar bond strength values in both cases, but significantly lower compared to their sequential application.Type
info:eu-repo/semantics/articleRights
Attribution-NonCommercial-ShareAlike 4.0 InternationalLanguage
engEISSN
20734360ae974a485f413a2113503eed53cd6c53
10.3390/polym14204291
Scopus Count
Collections
The following license files are associated with this item:
- Creative Commons
Except where otherwise noted, this item's license is described as Attribution-NonCommercial-ShareAlike 4.0 International