dc.identifier.citation1. Avila Solis, SM. Evaluación in vitro de la microrugosidad superficial de dos resinas tipo Bulk Fill inmersas a dos bebidas rehidratantes con pH de 2,79 y 3,3 [Internet]. [Lima, Perú]: Universidad Peruana de Ciencias Aplicadas(UPC).; 2019. Disponible en: http://hdl.handle.net/10757/628127
dc.identifier.urihttp://hdl.handle.net/10757/628127
dc.description.abstractObjetivo: Comparar in vitro la rugosidad superficial de una resina compuesta tipo BulkFill: Aura® BulkFill (SDI) con la resina Tetric N-Ceram® BulkFill (Ivoclar Vivadent) al ser inmersas a dos bebidas rehidratantes: Sporade® y Gatorade®. Materiales y métodos: Se utilizaron 88 especímenes de resina divididos en cuatro grupos, confeccionados con una matriz metálica (10mm x 4mm). Se insertó las resinas con una espátula de resina, y se fotoactivó con la lámpara Elipar LedTM, con una intensidad de 1200 mW/cm2. Se sumergieron los especímenes en agua destilada. A las 24 horas, se midió la rugosidad con el rugosímetro Mitutoyo SJ-210P. Luego, se realizó la inmersión en bebidas rehidratantes y se midió la rugosidad final a los 7 días. Resultados: La rugosidad inicial y final de las resinas Aura® BulkFill (SDI) y Tetric N-Ceram® BulkFill (Ivoclar Vivadent) presentaron diferencias significativas después de la inmersión en bebidas rehidratantes. Para los especímenes de Aura® BulkFill (SDI) al someterla a Sporade® se encontró una media inicial de 1.20 y una media final de 1.76 y los valores para Gatorade® fueron 0.77 y 1.73. Mientras que la rugosidad superficial de Tetric N-Ceram® BulkFill (Ivoclar Vivadent) al sumergirla en Sporade® fue 0.82 y 1.55, y en Gatorade® 0.77 y 1.73. Al comparar la diferencia de la rugosidad superficial final e inicial (deltas), la resina Aura® BulkFill presentó diferencias significativas mientras que, Tetric N-Ceram® BulkFill no tuvo diferencias al sumergirlas en ambas bebidas rehidratantes. Conclusiones: Las resinas estudiadas incrementaron su rugosidad luego de ser inmersas a las bebidas mencionadas.en_US
dc.description.abstractObjective: To compare in vitro the surface roughness of a BulkFill composite resin: Aura® BulkFill (SDI) with Tetric N-Ceram® BulkFill resin (Ivoclar Vivadent) when immersed in two rehydration drinks: Sporade® and Gatorade®. Materials and methods: 88 resin specimens divided into four groups were used, with a metal matrix (10 mm x 4 mm). The resins were inserted with a resin spatula, and photo-activated with the Elipar LedTM lamp, with an intensity of 1200 mW/cm2. The specimens were immersed in distilled water. After 24 hours, the roughness was measured with the Mitutoyo SJ-210P rugosimeter. Then, the immersion in rehydration drinks was performed and the final roughness was measured after 7 days. Results: The initial and final roughness of the resins Aura® BulkFill (SDI) and Tetric N-Ceram® BulkFill (Ivoclar Vivadent) showed significant differences after immersion in rehydration drinks. For specimens of Aura® BulkFill (SDI) when subjected to Sporade® an initial mean of 1.20 and a final average of 1.76 was found and the values for Gatorade® were 0.77 and 1.73. While the surface roughness of Tetric N-Ceram® BulkFill (Ivoclar Vivadent) when immersed in Sporade® was 0.82 and 1.55, and in Gatorade® 0.77 and 1.73. When comparing the difference of the final and initial surface roughness (deltas), the Aura® BulkFill resin showed significant differences while, Tetric N-Ceram® BulkFill did not have differences when immersing them in both rehydration drinks. Conclusions: The resins studied increased their roughness after being immersed in the aforementioned beverages.en_US
dc.description.uriTesises_PE
dc.formatapplication/pdfen_US
dc.formatapplication/epuben_US
dc.formatapplication/msworden_US
dc.language.isospaen_US
dc.publisherUniversidad Peruana de Ciencias Aplicadas (UPC)en_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.rightsAttribution-NonCommercial-ShareAlike 4.0 International*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-sa/4.0/*
dc.sourceUniversidad Peruana de Ciencias Aplicadas (UPC)es_PE
dc.sourceRepositorio Académico - UPCes_PE
dc.subjectResinas compuestasen_US
dc.subjectRugosidaden_US
dc.subjectBebidas rehidratantesen_US
dc.subjectComposite resinen_US
dc.subjectRoughnessen_US
dc.subjectSoft drinksen_US
dc.titleEvaluación in vitro de la microrugosidad superficial de dos resinas tipo Bulk Fill inmersas a dos bebidas rehidratantes con pH de 2,79 y 3,3en_US
dc.title.alternativeIn vitro comparison of superficial microroughness of two Bulk Fill resins composites inmersed into two soft drinksen_US
dc.typeinfo:eu-repo/semantics/bachelorThesisen_US
thesis.degree.grantorUniversidad Peruana de Ciencias Aplicadas (UPC). Facultad de Ciencias de la Saludes_PE
thesis.degree.levelLicenciaturaes_PE
thesis.degree.disciplineOdontologíaes_PE
thesis.degree.nameCirujano dentistaes_PE
refterms.dateFOA2019-12-01T18:46:59Z
dc.identifier.isni0000 0001 2196 144X
renati.typehttp://purl.org/pe-repo/renati/type#tesises_PE
renati.levelhttp://purl.org/pe-repo/renati/nivel#tituloProfesionales_PE
dc.publisher.countryPEes_PE
dc.type.otherTesises_PE


Files in this item

Thumbnail
Name:
AvilaS_S.pdf
Size:
677.4Kb
Format:
PDF
Thumbnail
Name:
AvilaS_S_Ficha.pdf
Embargo:
2089-10-21
Size:
1.062Mb
Format:
PDF
Thumbnail
Name:
AvilaS_S.docx
Embargo:
2089-10-21
Size:
1.499Mb
Format:
Microsoft Word 2007

This item appears in the following Collection(s)

Show simple item record

info:eu-repo/semantics/openAccess
Except where otherwise noted, this item's license is described as info:eu-repo/semantics/openAccess